Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 165N - PS - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 165N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Styrolution® PS 165N is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 3.4 cm³/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
Density of melt 936 kg/m³ -
Thermal conductivity of melt 0.155 W/(m K) -
Spec. heat capacity of melt 2300 J/(kg K) -
Ejection temperature 82 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3300 MPa ISO 527
Stress at break 52 MPa ISO 527
Strain at break 2 % ISO 527
Tensile creep modulus, 1h 3300 MPa ISO 899-1
Tensile creep modulus, 1000h 2600 MPa ISO 899-1
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 90 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 76 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 84 °C ISO 75-1/-2
Vicat softening temperature, B 89 °C ISO 306
Coeff. of linear therm. expansion, parallel 80 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.2 mm -
Yellow Card available yes - -
Oxygen index 18 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 2.5 - IEC 62631-2-1
Relative permittivity, 1MHz 2.5 - IEC 62631-2-1
Dissipation factor, 100Hz 0.9 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 0.7 E-4 IEC 62631-2-1
Comparative tracking index 375 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1040 kg/m³ ISO 1183
Material specific propertiesValueUnitTest Standard
ISO Data
Viscosity number 119 cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 230 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Diagrams
Viscosity-shear rate , Styrolution® PS 165N, PS, INEOS Styrolution
Shearstress-shear rate , Styrolution® PS 165N, PS, INEOS Styrolution
Stress-strain , Styrolution® PS 165N, PS, INEOS Styrolution
Secant modulus-strain , Styrolution® PS 165N, PS, INEOS Styrolution
Stress-strain (isochronous) 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Creep modulus-time 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Creep curve 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Specific volume-temperature (pvT) , Styrolution® PS 165N, PS, INEOS Styrolution
Tensile modulus-temperature , Styrolution® PS 165N, PS, INEOS Styrolution
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
Transparent
Regional Availability
Europe, Near East/Africa
Other text information
Injection molding
PROCESSING
injection molding, Melt temperature, range: 180 - 280 °C
injection molding, Melt temperature, recommended: 230 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 165N can be injection molded at temperatures between 180 and 280°C.Recommended mold temperatures are between 10 and 60°C.
Film extrusion
PROCESSING
Extrusion, Blown film, Melt temperature: 180 - 210 °C
Extrusion, Flat film, Melt temperature: 200 - 240 °C

Extrusion melt temperature should not exceed 240°C.
Other extrusion
PROCESSING
Extrusion, Pipes, Melt temperature: 180 - 210 °C
Profile extrusion
PROCESSING
Extrusion, Profiles, Melt temperature: 210 °C
Sheet extrusion
PROCESSING
Extrusion, Plates, Melt temperature: 200 - 230 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.